ISO 10363:1992
p
ISO 10363:1992
18423
недоступно на русском языке

Тезис

 Preview

The method is based on placing a stainless steel or glass vessel in an oil bath or oven, adding a sufficient quantity of the adhesive to the vessel, melting the sample, measuring the viscosity at the operating temperature and the softening point, repeating these operations at regular time intervals of between 4 h and 6 h, until the time for stopping the test according to pre-determined criteria is reached, and observing and recording, at the time that each measurement is taken, the following phenomena: skin formation, fumes, phase separation, gelation, change in colour.


Общая информация 

  •  : Опубликовано
     : 1992-12
  •  : 1
  •  : ISO/TC 61/SC 11 Products
  •  :
    83.180 Adhesives

Приобрести данный стандарт

ru
Формат Язык
std 1 40 PDF
std 2 40 Бумажный
  • CHF40

Жизненный цикл

Появились вопросы?

Ознакомьтесь с FAQ

Работа с клиентами
+41 22 749 08 88

Часы работы:
Понедельник – пятница: 09:00-12:00, 14:00-17:00 (UTC+1)