Тезис
Specifies the particular test conditions for determining the Vicat softening temperature of ABS and ASA pipes and fittings (the general test method is given in ISO 2507-1). Also gives, for information, the corresponding basic specifications.
Общая информация
-
Текущий статус: ОпубликованоДата публикации: 1995-02Этап: Международный стандарт подлежит пересмотру [90.92]
-
Версия: 1
-
Технический комитет :ISO/TC 138/SC 5
- RSS обновления
Новая версия в процессе разработки

Draft
International StandardISO/DIS 2507
Thermoplastics pipes and fittings — Vicat softening temperature: General test method and test conditions for Vinyl chloride - based (PVC-U, PVC-C, PVC-Hi) and Acryl nitrile - based (ABS, ASA) pipes and fittings
Reference number
ISO/DIS 2507
ISO/DIS 2507
Edition 1
© ISO 2025
Проект Международный стандарт
ISO/DIS 2507
Thermoplastics pipes and fittings — Vicat softening temperature: General test method and test conditions for Vinyl chloride - based (PVC-U, PVC-C, PVC-Hi) and Acryl nitrile - based (ABS, ASA) pipes and fittings
Part 3: Test conditions for acrylonitrile/butadiene/styrene (ABS) and acrylonitrile/styrene/acrylic ester (ASA) pipes and fittings
Жизненный цикл
-
Сейчас
ОпубликованоISO 2507-3:1995
Стандарт, который пересматривается каждые 5 лет
Этап: 90.92 (Будет пересмотрено)-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
-
00
-
Будет заменено
В стадии разработкиISO/DIS 2507