ISO 4662:2009 specifies two methods for determining the rebound resilience of rubber the hardness of which lies between 30 IRHD and 85 IRHD. They are the pendulum method and the tripsometer method.
With the pendulum method, a mass with a spherical end impacts a flat test piece, firmly held but free to bulge. The kinetic energy of the impacting mass is measured immediately before and after impact.
With the tripsometer method, a flat test piece is impacted by a hemisphere mounted on the periphery of a disc which is supported on an axle and caused to rotate by an off-axis mass. The kinetic energy of the impacting mass is measured immediately before and after impact.
Общая информация
-
Текущий статус: ОтозваноДата публикации: 2009-08Этап: Отмена международного стандарта [95.99]
-
Версия: 3
-
Технический комитет :ISO/TC 45/SC 2ICS :83.060
- RSS обновления
Жизненный цикл
-
Ранее
ОтозваноISO 4662:1986
-
Сейчас
-
00
Предварительная стадия
-
10
Стадия, связанная с внесением предложения
-
20
Подготовительная стадия
-
30
Стадия, связанная с подготовкой проекта комитета
-
40
Стадия, связанная с рассмотрением проекта международного стандарта
-
50
Стадия, на которой осуществляется принятие стандарта
-
60
Стадия, на которой осуществляется публикация
-
90
Стадия пересмотра
-
95
Стадия, на которой осуществляется отмена стандарта
Исправления
Исправление текущего издания; предоставляются бесплатно; не включены в текст действующего стандарта.ОтозваноISO 4662:2009/Cor 1:2010
-
00
-
Пересмотрен
ОпубликованоISO 4662:2017